can be calculated by the finite element method of stress magnitude different speeds to simulate the failure process and improve the design.
2013年8月26日星期一
Parts synthetic diamond powder molding method
Dissolved in a solvent of an organic binder and a modifier consisting of plastic media is mixed with the metal powder. cutting tools a solvent soluble at room temperature and at higher temperatures decreased solubility characteristics. Having a grinding wheel the performance ratio, the plastic medium is mixed with the metal powder, under pressure into the closed mold; heating mold cavity in the plastic and keep a constant Diamond blade increase in viscosity of the medium. Results adobe bonding by plastic media which may emerge from the mold cavity. Heated mold can remove some of the solvent, and then in the furnace hot manipulation solvent evaporation, leaving the body of the network pore pressure and the powder particles in contact with the adhesive film.